Study reveals inconsistency in nanoindentation testing using different Berkovich indenters

Date 22nd, Aug 2023
Source Phys.org - Scientific News Websites

DESCRIPTION

Nanoindentation testing is a high-precision instrumented indentation test technique that has the advantages of non-destructive testing and simplicity. However, researchers found that when testing the same sample with different Berkovich indenters, inconsistency still arises even if the indenters are regularly calibrated. This inconsistency poses challenges in accurately testing material hardness and comparing data from different laboratories.