An indium oxide-based transistor created using atomic layer deposition

Date 17th, Mar 2022
Source Tech Xplore - Scientific News Websites

DESCRIPTION

Over the past decades, engineers have created increasingly advanced and highly performing integrated circuits (ICs). The rising performance of these circuits in turn increased the speed and efficiency of the technology we use every day, including computers, smartphones and other smart devices.