Date4th, Sep 2019

Summary:

Scientists have discovered a new way to coat nuclear materials that supports efforts to minimize use of high-enriched uranium.

Full text:

Sep 04, 2019 Coating nuclear materials with atomic layer deposition (Nanowerk News) Inside an operating nuclear reactor, the environment is extreme, as reactor components are exposed to a combination of intense radiation and heat as well as chemically reactive coolant. Thats why, in order to operate reactors safely, scientists need to design their components with materials that can withstand these conditions. Researchers at the U.S. Department of Energys (DOE) Argonne National Laboratory have made a pivotal discovery by taking a technique originally developed for the semiconductor industry and using it as a way to coat nuclear materials. This technique, called atomic layer deposition (ALD), forms the basis of new methods to protect nuclear fuels and materials from direct exposure to the reactors hostile environment. Atomic layer deposition like its name suggests allows researchers to deposit atomically thin films of a particular material on a surface. By building up these layers, Argonne scientists can form chemically precise coatings designed to have a set of particular properties. We are pioneering the use of ALD for nuclear applications, said Argonne nuclear engineer Abdellatif Yacout, manager of the fuel development and qualification group. Argonne experts in the technique, led by Argonne Distinguished Fellow Michael Pellin, were instrumental in those advancements. Fuel coatings support efforts to minimize high-enriched uranium In one set of experiments, Argonne scientists have used ALD to deposit zirconium nitride (ZrN) as a coating directly over low-enriched uranium-molybdenum (U-Mo) powders. The coating is thin enough to allow neutrons to penetrate through, while shielding the fuel from degradation, generally from interaction with aluminum (Al), a major constituent of a research reactor fuel systems. Argonnes Sumit Bhattacharya (left) and Abdellatif Yacout (right) have discovered a new way to coat nuclear materials that support efforts to minimize use of high-enriched uranium. (Image: Argonne National Laboratory.) In order to study the stability of the newly developed ZrN coating and how it interacts with aluminum, scientists performed multiple ex situ irradiation studies using heavy ions (to simulate damage from fission fragments) at Argonnes Tandem Linac Accelerator System (ATLAS) facility, a DOE Office of Science User Facility. That specific work to redesign coatings for nuclear fuels supports the effort to convert high-power research reactors around the world that use high-enriched uranium (HEU) to use low-enriched uranium (LEU) fuels, in support of the national policy of HEU minimization. Coating claddings to hold up to reactor environments Two other sets of experiments involving ALD revolve around claddings, which are structural materials that encapsulate the fuel constituents inside of a nuclear reactor. High fretting resistance from a nano-laminate coating. This project used ALD to design cladding materials that would resist fretting wear, a behavior in reactor assemblies that contributes to mechanical wear. ?A way to resist fretting is to coat the surface of the cladding to increase its hardness, Yacout said. ?Cladding surfaces modified with an ALD coating (for example, aluminum oxide [Al2O3]) and followed by other treatments, increases the surface hardness by almost 100-fold. High temperature oxidation resistance. This project revolved around developing coating for claddings such that they can better withstand the high temperatures inside a reactor during severe accident conditions. The team developed a unique ceramic composite material, which can be fabricated at low temperature but with a significantly compact microstructure. Developing this ceramic-based composite coating is a two-step process. It involves combining electrophoretic deposition (EPD), a fast and low-temperature deposition method, with ALD. In this way, the Argonne researchers were able to quickly create a thick ceramic-ceramic composite coating that both adheres and conforms to the cladding surface. The power of a joint technique Neither EPD nor ALD as a deposition process by itself would have yielded a coating sufficient to protect the cladding, said Argonne researcher Sumit Bhattacharya. ?Even though ALD generates a pinhole-free, dense and adherent coating, the deposition rate is relatively slow. In order to deposit the thickness you need, it will take days or even in some cases weeks, he said. Meanwhile, if you only use EPD, the deposited layer is highly porous, and requires high-temperature sintering to become dense and adherent to the substrate. This is not ideal, as the cladding material is temperature-sensitive and it will lose all of its mechanical properties. One principal advantage of using the dual deposition techniques consists in the ability to greatly reduce the temperature needed to produce an adherent coating. Generally, to develop a dense ceramic composite, a high-temperature sintering step is necessary. However, because the cladding is made of metal, the typical sintering would cause the substrate to melt or lose its strength. Not only will you not achieve sintering, but the main substrate that you are trying to protect will be destroyed, Bhattacharya explained. The combination of the EPD/ALD technique achieves an adherent coating at a temperature of only around 300 degrees Celsius, far lower than the conventional sintering temperature required for such composites. Using ALD offers another essential benefit over other deposition techniques, such as chemical vapor deposition (CVD). Even though CVD deposits more quickly than ALD, in doing so it blocks parts of the channels that would need to be filled. As a result, it leaves behind large porosities inside the composite. ?Only ALD can make sure that we are able to treat all the nooks and crannies, Bhattacharya said. In order to test how the coating can endure the reactor irradiation environment, the researchers bombarded it with heavy ions at various temperatures in Argonnes Intermediate Voltage Electron Microscope facility (IVEM). Afterward, the sample stayed intact and scientists found no apparent changes in the nanopowder and the overlaying ALD coating. Source: Argonne National Laboratory addthis_logo = 'https://www.nanowerk.com/images/nwlogo200x50.gif'; addthis_logo_background = 'FFFFFF'; addthis_logo_color = '000066'; addthis_brand = 'Nanowerk'; addthis_options = 'favorites, delicious, tumblr, stumbleupon, google, live, more'; Subscribe to a free copy of one of our dailyNanowerk Newsletter Email Digests with a compilation of all of the day's news.

Source: